Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nye Lubricants 807 (FG) Synthetic Oil

Category Fluid , Lubricant , Polyalphaolefin (PAO) , PTFE Gellant
Manufacturer Nye Lubricants
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Nye Lubricants 807 (FG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 148
148
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 75 cSt
75 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 11 cSt
11 cSt
Base Oil; ASTM D445
Evaporation Loss 0.10 %
0.10 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 259
259
ASTM D217
Penetration P(60), 1/10 mm 274
274
ASTM D217
Oil Separation 0.50 %
0.50 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -54.0 °C
-65.2 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PAO
Gellant Type PTFE