Nye Lubricants 741E (NG) Synthetic Oil

Category Fluid , Lubricant , Lithium Gellant , Organic Soap Gellant , Silicone Base
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Nye Lubricants 741E (NG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 409
409
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 151 cSt
151 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 59 cSt
59 cSt
Base Oil; ASTM D445
Evaporation Loss 1.9 %
1.9 %
24 hrs, 150C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 446
446
ASTM D217
Penetration P(60), 1/10 mm 456
456
ASTM D217
Oil Separation 3.1 %
3.1 %
24 hrs, 150C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Recommended
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Recommended
Pour Point -60.0 °C
-76.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Sil.(Phenyl)
Gellant Type Li soap