Network Polymers NPP 50-0548

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 50-0548.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.1 MPa
3200 psi
ASTM D638
Elongation at Break 19 %
19 %
ASTM D638
Flexural Modulus 0.586 GPa
85.0 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature -70.0 °C
-94.0 °F