NOVA Chemicals Novapol® LE-0520-A LDPE Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF NOVA Chemicals Novapol® LE-0520-A LDPE Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: easy processing, good dispersion.Applications: Additive and color concentrates for film and molding.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Processing Properties Metric English Comments
Melt Temperature 180 - 225 °C
356 - 437 °F