Multibase Multi-Pro® 4002 C BLK 40% Filler Content Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 4002 C BLK 40% Filler Content Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This product is a high impact PP copolymer developed for extrusion applications. The product lends itself well for automation of nail-gun operation, requiring good melt strength and impact resistance.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792-91
Melt Flow 2.0 g/10 min
2.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 16.5 MPa
2390 psi
ASTM D638-95
Elongation at Break 200 %
200 %
ASTM D638-95
Flexural Modulus 1.655 GPa
240.0 ksi
Secant 1%; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Gardner Impact 7.90 J
5.83 ft-lb
ASTM D5420-93