Momentive Performance Materials Titanium Diboride/Boron Nitride Composite Vacuum Metallizing Boat

Category Ceramic , Boride , Ceramic Matrix Composite , Nitride
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Titanium Diboride/Boron Nitride Composite Vacuum Metallizing Boat.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Intermetallic composites from Advanced Ceramics are used vacuum metallizing industry. These ceramics withstand higher operating temperatures, have lower moisture sensitivity, low thermal expansion, and high density. Available in a selection of resistance ranges, IMC boats can be tailored to match available power supplies. These unique properties provide the vacuum metallizer a resistance heated source that operates at high evaporation levels, and is extremely durable in operation.Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.
Physical Properties Metric English Comments
Moisture Absorption 0.300 %
0.300 %
100% RH, 150 hours, RT
Mechanical Properties Metric English Comments
Flexural Strength 138 MPa
20000 psi
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C

@Temperature 20.0 °C
3.89 µin/in-°F

@Temperature 68.0 °F
Processing Properties Metric English Comments
Sintering Temperature 1900 °C
3450 °F
or higher