Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials RPC Boron Nitride (BN) Coating

Category Ceramic , Nitride , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RPC Boron Nitride (BN) Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is not recommended. Multiple coats may be necessary. Dried coatings can be readily handled, smoothed, or polished with a soft, dry cloth.Uses of Advanced Ceramics Corporation boron nitride water based coatings and aerosol spray: Release Agents, Lubricants and Protective Coatings Boron Nitride (BN) remains lubricious and inert even at extremely high temperatures. Coatings made with BN prevent sticking to increase the life of dies/molds, improve product surface finishes, and reduce production times.Metalforming In molten metal and metalforming applications, BN coatings protect surfaces which come in contact with hot and molten metals. BN inhibits corrosion and chemical attack and provides easier release and longer mold/die life. Applications include: casting, stamping, forging and powder metallurgy.Glass Making BN's high temperature lubricating properties make it ideal in glass making where it helps minimize surface defects, improve mold/die life and release, and reduce clean-up time. Most glass formulations will not stick to BN.Plastics/Rubber Producers of injection-molded plastics and elastomers benefit from BN die applications by improved die release and increased production speeds. Sintering Sintering of metallic and ceramic powders is typically done on graphite plates. A coating of BN can essentially eliminate carbon contamination, reactivity and sticking which can occur at sintering temperatures.Welding and Brazing BN coatings are also ideal for welding and furnace brazing. They protect surfaces from weld spatter and provide superior stop-off protection. BN coatings also protect MIG/MAG welding nozzles from weld spatter.Information provided by GE Advanced Ceramics.Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 550 °C
1020 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
typical (Boron Nitride Component)
Descriptive Properties Value Comments
% Solids Min 20%
Application Release, Protective Coating
Color White
Contents Binder BN Silicate
Dilution Yes
Dilution Amount 2:1
Relative Hardness 1
On a scale of 1-4 with 1 being the hardest.
Solvent Type Water