Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Micropol Microlink XL28/FR Black Crosslinkable Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Micropol Limited
Trade Name Microlink
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol Microlink XL28/FR Black Crosslinkable Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flame retardant. Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact), ESCR, chemical, and temperature resistance. It is fully UV stabilized and available in colors for outdoor use in all climates; minimum UV10 rating.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
M F50; ASTM D1693
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.0 MPa
3340 psi
50mm/min; ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.750 GPa
109 ksi
ASTM D790
Impact 36
36
J/mm, Micropol test based on ASTM D1790
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Brittleness Temperature <= -120 °C
<= -184 °F
ASTM D746
Flammability, UL94 HB
HB