Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Michem® Emulsion 43240 Polypropylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 43240 Polypropylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Polypropylene emulsionUsage: Michem® Emulsion 43240 is best used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is needed.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Volatiles 59.5 - 60.5 %
59.5 - 60.5 %
pH 7.5 - 9.5
7.5 - 9.5
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Amber, translucent liquid
Emulsifier Charge Nonionic
Solids Type Maleated Polypropylene