Michelman® Michem® Emulsion 21030 Anionic polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 21030 Anionic polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic polyethylene emulsionUsage: Michem® Emulsion 21030 provides abrasion resistance and anti-blocking properties as well as slip resistance when used as an additive in floor polish formulations.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Volatiles 69 - 71 %
69 - 71 %
pH <= 7.0
<= 7.0
Recommended pH of system
8.0 - 9.5
8.0 - 9.5
Brookfield Viscosity <= 50 cP
<= 50 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Tan liquid
Emulsifier Charge Anionic
Solids Type Polyethylene