Mateck Zinc Telluride, ZnTe

Category Ceramic , Sulfide/Chalcogenide , Other Engineering Material , Semiconductor
Manufacturer Mateck GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck Zinc Telluride, ZnTe.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Semiconductor single crystals. Twins and stacking faults twin free.
Physical Properties Metric English Comments
a Lattice Constant 6.1034 Ã…
6.1034 Ã…
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
undoped
Hole Mobility, cm²/V-s 130
130
Descriptive Properties Value Comments
Crystal Axis (111)
Density of low angle boundaries (cm^-1), max 10
EPD (cm^-2), MAX 500000
Orientation (100); (110); (111)
Orientation Accuracy ( ° ), Max 1
Polishing chemical mechanical polishing
one side or both sides polished
optical polishing
Production Method Markov
Standard Size (mm) 10 x 10 x 0.5 or 1
5 x 5 x 0.5 or 1
Structure cubic
Tolerance of Diameter (mm) 0.000 / -0.100
Tolerance of Length (mm) 0.05
Tolerance of Thickness (mm) 0.05