| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| a Lattice Constant | 4.758 Ã… | 4.758 Ã… | |
| c Lattice Constant | 12.99 Ã… | 12.99 Ã… |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.50 µm/m-°C | 4.17 µin/in-°F | |
| Melting Point | 2030 °C | 3690 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 9.0 | 9.0 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Dimensions (mm) | 10x10x0.5 | |
| Junction Angle ° | 24±1 | |
| Structure | hexagonal | |
| Surface Orientation ° | 1012±1 | |
| Surface Roughness (angstroms) | 10 | |
| max 50 |