Master Bond MB297MED Cyanoacrylate Biocompatible Adhesive System

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Master Bond MB297MED Cyanoacrylate Biocompatible Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Medical grade, Class VI approved, fills gap to 0.008Information provided by Master Bond Inc.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Viscosity 2400 cP

@Temperature 23.0 °C
2400 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Optical Properties Metric English Comments
Refractive Index 1.48
1.48
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
35-45°F
Descriptive Properties Value Comments
Color Transparent
Set-Up Time, minutes 0.33-0.833
At Room Temperature