Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MarkeTech Repton EXP 22 Magnesia MgO

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Repton EXP 22 Magnesia MgO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are available with a smooth or a unique textured surface that permits pinpoint contact with the load. Sticking can be eliminated as well as providing a surface that breathes, allowing gasses from the ceramic to escape.Applications include firing ceramic capacitors, SOFCs, PZTs, hard and soft ferrites, co-fired substrates and powdered metals. REPTON is available in a wide range of compositions that include a range of alumina, mullite/alumina, zirconia, cordierite, magnesia, and aluminum titanate.
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
Porosity 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Flexural Strength >= 89.0 MPa
>= 12900 psi
Thermal Properties Metric English Comments
CTE, linear 11.2 µm/m-°C

@Temperature 300 °C
6.22 µin/in-°F

@Temperature 572 °F
13.2 µm/m-°C

@Temperature 900 °C
7.33 µin/in-°F

@Temperature 1650 °F
Component Elements Properties Metric English Comments
MgO 100 %
100 %
Descriptive Properties Value Comments
Spall Resist 350°C
Copyright © lookpolymers.com All Rights Reserved