Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MarkeTech Repton 914 Magnesia MgO

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF MarkeTech Repton 914 Magnesia MgO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are available with a smooth or a unique textured surface that permits pinpoint contact with the load. Sticking can be eliminated as well as providing a surface that breathes, allowing gasses from the ceramic to escape.Applications include firing ceramic capacitors, SOFCs, PZTs, hard and soft ferrites, co-fired substrates and powdered metals. REPTON is available in a wide range of compositions that include a range of alumina, mullite/alumina, zirconia, cordierite, magnesia, and aluminum titanate.
Physical Properties Metric English Comments
Bulk Density 3.10 g/cc
0.112 lb/in³
Density 3.48 g/cc
0.126 lb/in³
calculated from bulk density after subtracting pore volume
Porosity 11 %
11 %
Mechanical Properties Metric English Comments
Flexural Strength >= 98.0 MPa
>= 14200 psi
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 300 °C
6.67 µin/in-°F

@Temperature 572 °F
14.0 µm/m-°C

@Temperature 900 °C
7.78 µin/in-°F

@Temperature 1650 °F
Component Elements Properties Metric English Comments
MgO 100 %
100 %
Descriptive Properties Value Comments
Spall Resist 300°C
Users viewing this material also viewed the following: