MV Labs SM900 SmPO4.xH2O Samarium phosphate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs SM900 SmPO4.xH2O Samarium phosphate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 246.41 g/mol
246.41 g/mol
Descriptive Properties Value Comments
CAS Number 13465-57-1
Form Yellow powder
Purity 99.99%
Typical Impurities Check with Manufacturer