MV Labs IR800 IrO2 Iridium(IV) oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs IR800 IrO2 Iridium(IV) oxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 224.2 g/mol
224.2 g/mol
Descriptive Properties Value Comments
Assay 86% Ir
CAS Number 12030-49-8
Form Black powder
Purity 99.99%
Typical Impurities Na < 50; Rh < 20; Ag, Ca, Pd < 8; Rh, Al, Fe, Zn < 3 ppm