M. Holland Company PC522UR Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer M. Holland Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company PC522UR Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High flowHigh impact resistanceGood mold releaseGood UV resistanceApplications: AppliancesProtective coveringsDecorative displaysHousings
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
23/23°C; ASTM D792
Melt Flow 22 g/10 min
22 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.2 MPa
9600 psi
ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
(0.125 in); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 139 °C
282 °F
Annealed; ASTM D648
Descriptive Properties Value Comments
Characteristics Mold release, UV stabilizer
Forms Pellets
Processing Methods Injection molding