LyondellBasell Petrothene® NA217000 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA217000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsPETROTHENE NA 217-000 is a high speed, lightweight coating resin for use with paper, films and other base stocks. This resin can yield coating weights down to 3.5 lbs/ream at line speeds of 1200 ft./min. or higher. Products made from materials coated with NA 217-000 include flexible packaging, milk cartons, industrial papers and foil mounting, single-ply bags, pouch bags, board trays, fiber drums, corrugated boxes and fiberboard containers. Regulatory StatusNA 217-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesNA 217-000 can be applied to paper, foil, cellophane, polyester film and other base stocks by conventional extrusion coating processes. The maximum recommended melt temperature is 625°F. For further recommendations, contact your Equistar sales representative. Physical PropertiesThese are typical values and not to be construed as specific product limits.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Water Vapor Transmission 7.80 g/m²/day
0.502 g/100 in²/day
ASTM E96
Melt Flow 5.6 g/10 min
5.6 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength at Break 12.4 MPa
1800 psi
Type IV specimen; ASTM D638
Elongation at Break 550 %
550 %
Type IV specimen; ASTM D638
Flexural Stiffness 276 MPa
40000 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525