LyondellBasell Aquathene® AQ120000 Ethylene Vinylsilane Copolymer

Category Polymer , Thermoplastic
Manufacturer LyondellBasell (former Equistar)
Trade Name Aquathene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Aquathene® AQ120000 Ethylene Vinylsilane Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsAQUATHENE AQ 120-000 is an ethylene vinylsilane copolymer designed for use in low voltage, power cable applications. This natural resin can be crosslinked, by exposure to moisture after extrusion with an appropriate catalyst.Processing TechniquesAQ 120-000 can be extruded using conventional extrusion equipment. For example, AQ 120-000 has been extruded successfully using a 2.5", 20:1 extruder equipped with a Maddock mixing screw under suggested temperature conditions. Regulatory StatusCrosslinking of the total system, AQ 120-000 and an appropriate crosslinking catalyst such as AQUATHENE CM 04482, occurs after the materials are mixed during extrusion and exposed to moisture. Crosslinking can be achieved by exposure to steam, immersion in hot water or storage at ambient conditions. The time required to achieve crosslinking depends on the catalyst masterbatch and temperature of the moisture. Because conditions can vary considerably, contact your Equistar sales representative for detailed recommendations. AQ 120-000 should be stored separately from the crosslinking catalyst masterbatch unitl extrusion. This resin can be stored in bulk for several months without special packaging and should not require drying prior to extrusion.Physical PropertiesAll properties determined from compression molded plaques. The values listed for physical electrical properties are nominal only and are subject to normal variations consistent with the test methods and/or variations found acceptable to the industry.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.2 MPa
1920 psi
ASTM D638
Elongation at Break 720 %
720 %
ASTM D638
Processing Properties Metric English Comments
Feed Temperature 154 °C
310 °F
Zone 2 163 °C
325 °F
Zone 3 168 °C
335 °F
Zone 4-x 177 °C
350 °F
Adapter Temperature 177 °C
350 °F
Die Temperature 177 °C
350 °F