Material Notes:
Adhesive resin Lushan EP252 is maleic grafted polyethylene. It’s mainly used for reinforced PE spiral corrugated steel pipes and steel wire with larger caliber. Adhesive resin Lushan EP252 solves the adherence problems between plastics and plastics, plastics and metal, glass and other materials. With super strong adhesion, wide application scope, excellent water and oxygen insulating properties, adhesive resin Lushan EP252 series provides a comprehensive solution for larger diameter steel pipe in drainage and sewerage pipe systems.Information provided by Lushan
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Melt Index of Compound 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Brittleness Temperature -70.0 °C
-94.0 °F
ASTM D746