Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® CR180A Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® CR180A Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ASTM D412
Tensile Strength, Yield 4.90 MPa
711 psi
at 100% elongation; ASTM D412
8.34 MPa
1210 psi
at 300% elongation; ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Tear Strength 88.3 kN/m
504 pli
Die C; ASTM D624
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
50 %

@Temperature 70.0 °C,
Time 79200 sec
50 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 70.0 °C
158 °F
ASTM D1525