Lubriplate SPO-277 Petroleum-Based Gear, Bearing, & Recirculating Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate SPO-277 Petroleum-Based Gear, Bearing, & Recirculating Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubrication for high sliding action in worm gears. They are also excellent for bevel, helical, and spur gears. They can be used with silver alloy, copper, and copper alloy bearings. Excellent for use in high moisture and high temperature applications. Provides performance comparable to synthetic lubricants. SPO Series Oils are available in Bottles, Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 101
101
Viscosity Index
460
460
ISO Grade
Saybolt Viscosity at 100°F 2260 SUS
2260 SUS
Saybolt Viscosity at 210°F 148 SUS
148 SUS
Kinematic Viscosity at 40°C (104°F) 432 cSt
432 cSt
Kinematic Viscosity at 100°C (212°F) 30 cSt
30 cSt
Thermal Properties Metric English Comments
Pour Point -9.44 °C
15.0 °F
Flammability Test 580
580
[°F] Fire Point
Flash Point 246 °C
475 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 140
SAE No. 70