Lubriplate SFL-2 Aluminum Complex Synthetic Food Machinery Grade Grease

Category Fluid , Lubricant , Aluminum Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate SFL-2 Aluminum Complex Synthetic Food Machinery Grade Grease.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This series provides an exceptionally wide operating temperature range, high shear stability, excellent water resistance, and load carrying properties. For use in freezers and other cold temperature applications or in areas subject to both cold and elevated temperatures. Available in 4 densities.SFL Series are available in Cartridges, Pails, 1/4 Drums & Drums.H-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1070 SUS
1070 SUS
Kinematic Viscosity at 40°C (104°F) 219 cSt
219 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 265
265
Unknown Amount of Work
Penetration P(60), 1/10 mm 295
295
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -31.7 °C
-25.0 °F
Approx. Cold test
Dropping Point 260 °C
500 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW
NLGI Grade 2
Rust/Oxidative Additives YES
Water Resistant YES