Lord Adhesives Chemglaze® 9956 Airless Spray Thinner

Category Fluid , Solvent
Manufacturer Lord Adhesives
Trade Name Chemglaze®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Chemglaze® 9956 Airless Spray Thinner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemglaze® thinners are formulated with urethane grade solvents and are used to reduce viscosity, aid bubble release, minimize orange peel, and make application easier.Chemglaze 9974 additive is used for bubble release when using a roller in some Chemglaze Z-Line and V-Line coatings.A blend of slow evaporating, aromatic solvents for improved leveling and flow out, especially for airless spray. Slow evaporation rate and low solvency. Normal use is 10% or less.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
Thermal Properties Metric English Comments
Flash Point 52.2 °C
126 °F
Seta, Closed Cup
Electrical Properties Metric English Comments
Surface Resistance 1.05e+7 ohm
1.05e+7 ohm
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 0.000 - 32.0 °C
12.0 Month

@Temperature 32.0 - 89.6 °F
Descriptive Properties Value Comments
Appearance Clear to straw yellow