Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® SpeedBonder™ 325 High Temperature Acrylic Bonding Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name SpeedBonder™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® SpeedBonder™ 325 High Temperature Acrylic Bonding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. On contact with an activator, these no-mix materials cure rapidly at room temperature to a weather-resistant bond. Bonding Type: Acrylic Typical Use: High temperature applications
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Viscosity 20000 cP
20000 cP
at 20 RPM
Mechanical Properties Metric English Comments
Adhesive Bond Strength 15.2 MPa
2200 psi
Varies with substrates
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Color Amber
Gap Fill 0.04 in.
Users viewing this material also viewed the following: