Material Notes:
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designed specifically for the assembly of medical devices where toxicity testing and sterilization resistance are required.Loctite® 4601 Cyanoacrylate Adhesive Key Substrates: Thermoplastic, thermoset plastic, metal Cure Type: Moisture
Physical Properties Metric English Comments
Brookfield Viscosity 50 cP

@Temperature 25.0 °C
50 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Descriptive Properties Value Comments
Color Clear