BCC Products BC 83 Liquid Wax Painting/White

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 83 Liquid Wax Painting/White.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BC83 Liquid Wax Parting/White is an excellent low viscosity, easy to use release agent for two component epoxy and polyurethane systems. Rigid, semi-rigid and flexible parts release from molds easily and fine surface detail is achieved. Features: Can be used on most common mold surfaces (plaster surfaces must be dry before application). It is specifically compounded for use with polyurethane systems, but it can be used with epoxy and polyester systems as well. Minimal film thickness will give maximum results. Polishes out smoothly for fine surface reproduction, unlimited shelf life, freeze/thaw stable and mild odor.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.755 g/cc
0.755 g/cc
pH 7.0
7.0
Thermal Properties Metric English Comments
Flash Point 40.6 °C
105 °F
Descriptive Properties Value Comments
Appearance milky white liquid