Material Notes:
LGflex BET is the new material developed by LG for the time in the world. Certified as a product that conforms to the standards of 21 CFR (FDA) and 16 CFR (Acute Oral Toxicity) of the code of federal regulations in the US. LGflex BET is an environment-friendly (non-endocrine disrupter) plasticizer for PVC soft sheet and injection, with excellent volatile resistance, migration resistance and improved odor qualities.Application: Non-toxic Sheets, Toys, Interior and External Decoration of AutomobilesCSA No. 610787-76-3Information provided by LG Chemical
Physical Properties Metric English Comments
Molecular Weight 490 g/mol
490 g/mol
Thermal Properties Metric English Comments
Melting Point -41.0 °C
-41.8 °F
Freezing Point
Boiling Point 346 °C

@Pressure 0.101 MPa
655 °F

@Pressure 14.7 psi
Chemical Properties Metric English Comments
Acid Value <= 0.10

@Treatment Temp. 125 °C,
Time 10800 sec
<= 0.10

@Treatment Temp. 257 °F,
Time 3.00 hour
After Heating, KOH mg/g; JIS K6751
Descriptive Properties Value Comments
Acidity <0.1 KOH mg/g
JIS K6751
Color <150 APHA
JIS K6751