Material Notes:
Description: Cariflex IR0307 KU polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its Logarithmic Inherent Viscosity (LIV) value of 6.80 dl/g. It is supplied from North America in the physical form identified: Cariflex IR0307 KU - supplied as white/transparent solid baleRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: A non-staining stabilizer is added at the typical value of 0.1%. Cariflex IR0307 KU polymer is manufactured to the highest standards but special requirements apply to certain sensitive applications such as food contact and pharmaceuticals. Reference should always be made to local legislation regulating these applications. Cariflex IR0307 KU Polymer is used as a replacement for natural rubber in a wide range of compounds, offering advantages of light color, uniformity and low levels of impurities. Its good flow characteristics produce improvements in mixing and molding behavior. It is used for food and pharmaceutical packaging and seals, baby bottle teats and health care, adhesives, chemical derivatives of rubbers and very light colored or transparent articles.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Medical; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Ash <= 0.10 %
<= 0.10 %
KM 35
Mechanical Properties Metric English Comments
Tensile Strength >= 21.6 MPa
>= 3130 psi
Cure: 40 mins at 135°C; ISO 37
Elongation at Break >= 428 %
>= 428 %
Cure: 40 mins at 135°C; ISO 37
300% Modulus 0.00860 - 0.0135 GPa
1.25 - 1.96 ksi
Cure: 40 mins at 135°C; ISO 37
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Content 1,4-Cis, FTIR
>90%, KM 34
1,4-Cis, NMR
>82%, KM 34
LIV
6.0-7.6 dL/g, KM 33
LVN
6.7-9.2 dL/g, KM 33
Stabilizer
0.06-0.12%, KM 31