Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 35 µm)

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Kinlead
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 35 µm).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has corona treatment. It is widely used in food and gift packaging for metallization.Information provided by Kinlead.
Physical Properties Metric English Comments
Thickness 35.0 microns
1.38 mil
± 2.5%; ASTM-252-78
Linear Mold Shrinkage 0.040 cm/cm
0.040 in/in
ASTM-D1204
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ASTM-D1204
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
ASTM-D882
Film Elongation at Break, TD 60 %
60 %
ASTM-D882
Coefficient of Friction 0.45
0.45
T/T-US; ASTM-D1894
0.50
0.50
T/O-US; ASTM-D1894
Film Tensile Strength at Break, MD 160 MPa
23200 psi
ASTM-D882
Film Tensile Strength at Break, TD 305 MPa
44200 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 1.2 %
1.2 %
ASTM-D1003
Gloss 94 %
94 %
ASTM-D2457
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Wetting Tension (Dyn) 39
ASTM-D2578
Yield (m²/kg) 31.4
Kinlead