Karina E 680D48/1-G-IS Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Karina E 680D48/1-G-IS Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.45 g/cc
1.39 - 1.45 g/cc
ASTM D 792
ASTM Color -1.84 - 1.16
-1.84 - 1.16
Color A, ME 12
-1.53 - 1.47
-1.53 - 1.47
Color B, ME 12
26.24 - 29.24
26.24 - 29.24
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 66 - 70

@Time 15.0 sec
66 - 70

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 7.85 MPa
>= 1140 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application Automotive Wires/Cables for General Purposes