Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.26 g/cc
1.20 - 1.26 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62

@Time 15.0 sec
58 - 62

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 6.37 MPa
>= 925 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638
Descriptive Properties Value Comments
Application Packaging/Stopper Seals