Karina 806-10/236-H-ISE White PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Karina 806-10/236-H-ISE White PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
ASTM 792
ASTM Color -2.19 - -0.190
-2.19 - -0.190
Color B, ME 12
-1.57 - 0.43
-1.57 - 0.43
Color A, ME 12
90.24 - 92.24
90.24 - 92.24
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 10.0 MPa
>= 1450 psi
ASTM D 638
>= 10.0 MPa
>= 1450 psi
After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
>= 200 %
>= 200 %
After 168H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application Coaxial