Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) TG 641 Super Bright Polyethylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) TG 641 Super Bright Polyethylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polyethylene Terephthalate fiber grade chips, super brightApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Viscosity Test 63 - 65 cm³/g
63 - 65 cm³/g
Ubbelhode
Thermal Properties Metric English Comments
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Processing Properties Metric English Comments
Moisture Content <= 0.25 %
<= 0.25 %
Karl-Fisher