Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) SBR-1500 Styrene Butadiene Rubber

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) SBR-1500 Styrene Butadiene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SBR–1500 is a high molecular weight styrene butadiene rubber combining good extrusion behavior and superior compound properties. SBR 1500 contains antioxidant to avoid product degradation. The high strength and great toughness of rubber permit the use of its elastic qualities. The properties of rubber show excellent resistance to cutting, tearing and abrasion. It has a relatively long, useful life under a wide variety of conduction.Applications: tires, tread rubber, molded and extruded mechanical goods.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D1416
Viscosity Measurement 52
52
raw viscosity, ML 1+4 @ 100°C; ASTM D1646
<= 84
<= 84
compound viscosity, ML 1+4 @ 100°C; ASTM D1646
Ash <= 1.5 %
<= 1.5 %
ASTM D1416
Mechanical Properties Metric English Comments
Tensile Strength >= 24.5 MPa
>= 3560 psi
35 min cured; ASTM D412
Elongation at Break 470 %
470 %
35 min cured; ASTM D412
300% Modulus 0.0136 GPa
1.98 ksi
35 min cured; ASTM D412
Chemical Properties Metric English Comments
Styrene Content 23.5 %
23.5 %
ASTM D1416
Descriptive Properties Value Comments
Organic Acid, % 6.125
ASTM D1416
Soap, % < 0.5
ASTM D1416
Copyright © lookpolymers.com All Rights Reserved