Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 1196NN Polypropylene Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER UNREINFORCED, CONTAIN FLAME RETARDANT, UL 94 V-2 APPROVAL, HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D785
Tensile Strength, Yield 30.4 MPa
4410 psi
ASTM D638
Elongation at Break 21 %
21 %
ASTM D638
Flexural Yield Strength 41.2 MPa
5970 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 0.441 J/cm

@Temperature 23.0 °C
0.827 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648