Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ICO Polymers ICORENEâ„¢ 195-1330 LMDPE Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICORENE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICORENEâ„¢ 195-1330 LMDPE Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: ICORENE 195-1330 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key Characteristics: good physical properties, easy molding, controlled release. Key Characteristics: good physical properties, easy molding, controlled release. Applications: This ICORENE® grade is particularly suitable for use in general purpose applications. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ASTM D1505
Melt Index of Compound 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 20.99 MPa
3045 psi
50 mm/min; ASTM D638
Elongation at Break 500 %
500 %
50 mm/min; ASTM D638
Flexural Modulus 0.5499 GPa
79.75 ksi
1.3 mm/min; ASTM D790
Impact 23

@Temperature -20.0 °C
23

@Temperature -4.00 °F
J/mm, instrumented impact, rotomolded test sample; ICO R&D1.14
Descriptive Properties Value Comments
UV Light Weatherometer Test 8000 hours
ASTM G26
Users viewing this material also viewed the following: