Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG8X Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Bulk Density 3.00 g/cc
0.108 lb/in³
Density 14.60 g/cc
0.5275 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 93.2
93.2
Tensile Strength, Ultimate 3500 MPa
508000 psi
Component Elements Properties Metric English Comments
Cobalt, Co 8.0 %
8.0 %
Other 1.5 %
1.5 %
WC 90.5 %
90.5 %
Descriptive Properties Value Comments
Flow Rate; sec/50g 24-30