Hong Kun Group UV 531 UV Absorber

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hong Kun Group UV 531 UV Absorber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chemical Name: 2-hydroxy-4-(octyloxy)benzophenoneCAS No. 1843-05-6All information provided by Hongkun Group
Physical Properties Metric English Comments
Loss On Ignition <= 0.10 %
<= 0.10 %
residue on ignition
Evaporation Loss <= 0.50 %
<= 0.50 %
loss on drying
Thermal Properties Metric English Comments
Melting Point 47.0 - 49.0 °C
117 - 120 °F
Optical Properties Metric English Comments
Transmission, Visible >= 92 %
>= 92 %
Descriptive Properties Value Comments
Appearance pale yellow crystalline powder
E (1.0%/1cm) 450-500
Purity (%) >= 99
GC