Hong Kun Group AO 1790 Antioxidant

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Hong Kun Group AO 1790 Antioxidant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chemical name: 1,3,5-tris(4-tert-butyl-3-hydroxy-2,6-dimethylbenzCAS No. 40601-76-1All information provided by Hongkun Group
Physical Properties Metric English Comments
Ash <= 0.50 %
<= 0.50 %
Thermal Properties Metric English Comments
Melting Point 159 - 163 °C
318 - 325 °F
Descriptive Properties Value Comments
Appearance offwhite powder