Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexWeb® HDC-660 - 3/16 - 17.5 (R2) Heavy Density Core

Category Other Engineering Material , Composite Core Material , Composite Fibers , Polymer , Thermoset , Carbon Fiber/Thermoset Composite
Manufacturer Hexcel
Trade Name HexWeb®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HDC-660 - 3/16 - 17.5 (R2) Heavy Density Core.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with either a thermoplastic or thermoset resin for the web impregnations. The product was developed for use in temperatures up to 500°F. Depending on the constituent resin system, the product may be suitable for short exposures at higher temperatures.Features: High compression strength non-metallic honeycomb available; Formability tailored to customer's needs; Low-moisture pickup; High thermal stability, very low coefficient of thermal expansion; Proven history in service; High corrosion resistance.Applications: HexWeb® HDC is used in sandwich structure as a replacement for potting compound in hard points or where extremely high compressive or shear strength is required. Using HexWeb® HDC in lieu of potting compound reduces process steps, improves part quality and reduces weight in the overall structure.
Physical Properties Metric English Comments
Density 0.280 g/cc
0.0101 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength 26.9 MPa
3900 psi
Stabilized
Shear Strength 7.58 MPa
1100 psi
Long Beam Shear, W Direction
13.4 MPa
1950 psi
Long Beam Shear, L Direction