Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexTow™ IM7 (5000) Carbon Fiber

Category Carbon , Carbon Fiber
Manufacturer Hexcel
Trade Name HexTow™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Hexcel® HexTow™ IM7 (5000) Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HexTow™ IM7 (HS-CP-5000) carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 6,000 (6K) and 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. HexTow™ IM7 (HS-CP-5000) fiber has shear properties equivalent to those of standard AS type fibers. It is suggested for use in prepregging and filament winding.The unique properties of HexTow™ IM7 (HS-CP-5000) fiber, such as higher tensile strength and modulus, as well as good shear strength, allow structural designers to achieve both higher safety margins for both stiffness and strength critical applications.Information provided by Hexcel
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Filament Diameter 5.2 µm
5.2 µm
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2760 MPa
400000 psi
Typical epoxy composite property
5480 MPa
795000 psi
Typical fiber property
Elongation at Break 1.8 %
1.8 %
6K; Calculated from tow test data
1.9 %
1.9 %
12K; Calculated from tow test data
Tensile Modulus 168 GPa
24400 ksi
Typical epoxy composite property
276 GPa
40000 ksi
Typical fiber property; Chord 6000-1000
Flexural Modulus 148 GPa
21500 ksi
Typical epoxy composite property
Shear Strength 128 MPa
18600 psi
Typical epoxy composite property; short-beam
Component Elements Properties Metric English Comments
Carbon, C 94 %
94 %
Descriptive Properties Value Comments
Approximate Yield (m/g) 2.24
12K
4.48
6K
Fiber Volume (%) 62
Tow Cross-Sectional Area (mm2) 0.13
6K
0.25
12K
Weight/Length (g/m) 0.223
6K
0.446
12K
Users viewing this material also viewed the following: