H.C. Starck Amperit® 704.1 Chromium Oxide (Cr2O3) 99.5%

Category Ceramic , Oxide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 704.1 Chromium Oxide (Cr2O3) 99.5%.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Particle Size 15 µm
15 µm
Maximum of 5% less than
62 µm
62 µm
Minimum of 95% less than
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Cr2O3 99.35 - 100 %
99.35 - 100 %
Fe2O3 <= 0.10 %
<= 0.10 %
SiO2 <= 0.25 %
<= 0.25 %
TiO2 <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Acid Soluble wt%, max 0.15