Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fujipoly Industries FLAT-5TV-12-.75 silicone rubber fusible tape

Category Polymer , Thermoset , Silicone
Manufacturer Fujipoly Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fujipoly Industries FLAT-5TV-12-.75 silicone rubber fusible tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Fujipoly Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 55
45 - 55
Tensile Strength, Ultimate >= 4.65 MPa
>= 674 psi
Elongation at Yield >= 400 %
>= 400 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
Moist
1.00e+15 ohm-cm
1.00e+15 ohm-cm
Normal
Dielectric Breakdown >= 4500 V
>= 4500 V
Withstand Voltage AC V
Descriptive Properties Value Comments
Adhesive Force, min, grams 300
Color Red