American Computer Optics Water White Filter 2 mm Single-Sided

Category Ceramic , Glass , Filter , Optical
Manufacturer American Computer Optics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Computer Optics Water White Filter 2 mm Single-Sided.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maximum Size: 75" X 110"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity exposure (50 C, 95% humidity)Solubility: The coated optical surface will show no signs of deterioration after a 24 hour immersion or exposure at room temperature (-60 F to + 90F) in each of the following solutions: Distilled Water - Acetone - Ethyl Alcohol - Isopropyl Alcohol - Trichloroethylene - 1.1.1 TrichlorethaneTempering AvailableInformation provided by American Computer Optics.
Physical Properties Metric English Comments
Thickness 2000 microns
78.7 mil
Optical Properties Metric English Comments
Transmission, Visible 99 %
99 %
Reflection Coefficient, Visible (0-1) <= 0.040
<= 0.040