Formosa Plastics Formolene® 1102KR Cast Film Polypropylene

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 1102KR Cast Film Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HomopolymerApplications: Cast film applications such as slit tape fabric stock and cordage.Formolene 1102KR is a highly isotactic polypropylene homopolymer designed primarily for cast film applications such as slit tape fabric stock and cordage. It contains a unique combination of stabilizers which give it low water carry over as well as excellent melt stability.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 4.0 g/10 min

@Temperature 230 °C
4.0 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256