Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

FloMet 17-4PH Stainless Steel, Heat Treated (H-900)

Category Metal , Ferrous Metal , Stainless Steel , Precipitation Hardening Stainless
Manufacturer FloMet LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF FloMet 17-4PH Stainless Steel, Heat Treated (H-900).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume metal powder and 40% volume plastic. The mixture (referred to as feedstock) is then injection molded at relatively low temperatures and pressures in conventional plastic injection molding machines. The molded green parts are then thermally processed in two steps. First, the binder is removed by evaporation in an operation called debinding. Next, the part is sintered in a dry hydrogen atmosphere, which densifies the part isotropically. The complex shape of the original molded part is retained throughout the process, and close tolerances can be achieved. Density is typically 95-98% of the wrought metal; mechanical properties and corrosion resistance are similar to wrought materialInformation provided by FloMet LLC.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 38 - 42
38 - 42
Tensile Strength, Ultimate 1280 MPa
185000 psi
Tensile Strength, Yield 1100 MPa

@Strain 0.200 %
160000 psi

@Strain 0.200 %
Elongation at Break 7.0 %
7.0 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Cb + Ta 0.30 %
0.30 %
Chromium, Cr 16.5 %
16.5 %
Copper, Cu 4.0 %
4.0 %
Iron, Fe 75 %
75 %
As remainder
Nickel, Ni 4.0 %
4.0 %