Flint Hills AP5106-HA Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills AP5106-HA Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Excellent impact stiffness balance, good mold release.Applications: Compression and injection molding: caps and closuresInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus, 1% Secant 1517 MPa
220000 psi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 9.00 J

@Temperature -30.0 °C
6.64 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1586 MPa
230000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648