Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fibre Glast Duratec 1040 Clear Hi-Gloss Gel Coat Additive

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer Fibre Glast Developments Corporation
Trade Name Duratec
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast Duratec 1040 Clear Hi-Gloss Gel Coat Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
#1040 can be mixed 1:1 with regular gel coat to reduce viscosity, porosity, and permit a complete open air cure. The reduction in viscosity allows gel coat to be sprayed controllably through siphon and HVLP equipment, reducing sanding and polishing time. Below the waterline repairs still need the addition of #71 Styrene Wax for maximum hardness. Features:Low Porosity - when used for repairs, blending the additive with gelcoat produces a low porosity surfaceReduced orange peel - the low viscosity of the blend results in a smooth finish that is easily sandedImproved properties - for mold surfaces, the blending of the additive with tooling gelcoat creates a higher heat distortion temperature, improved gloss retention, increased impact resistance and reduced subsurface porosity.Superior Finish - when blended one-to-one with gelcoats, the additive created an air-cure enamel-like coating. No air-dry additive is required. When used for gelcoat repair, surfaces are restored to like-new condition.Information provided by Fibre Glast Developments Corporation.
Physical Properties Metric English Comments
Brookfield Viscosity 110 cP
110 cP
Brookfield RVF #2 Spindle at 20 rpm
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Gel Time 16.0 - 20.0 min
16.0 - 20.0 min
Value for a 100g mass, catalyzed at 2 percent with MEKP - 2%
Users viewing this material also viewed the following: